DIN EN 15384-2
Packaging - Test method to determine the porosity of the internal coating of flexible aluminium tubes - Part 2: Copper sulphate test; German version EN 15384-2:2017
Packmittel - Prüfverfahren zur Bestimmung der Porosität der Innenbeschichtung von Aluminiumtuben - Teil 2: Kupfersulfatverfahren; Deutsche Fassung EN 15384-2:2017
Overview
This European Standard (EN 15384-2:2017) has been prepared by Technical Committee CEN/TC 261 "Packaging", the secretariat of which is held by AFNOR (France). The responsible national standardization committee is Working Committee NA 115-02-08 AA "Tuben" ("Tubes") of DIN Standards Committee Packaging (NAVp). This European Standard is applicable for internally coated cylindrical aluminium tubes, mainly used for the packing of pharmaceutical, cosmetic, hygiene, food or other household products. The internal coating is used as a barrier and should avoid any contact between aluminium and the product. This European Standard defines the copper sulphate method to detect the electrolyte conductivity as one criterion for the quality of the internal coating. The electrolyte conductivity of internally coated aluminium tubes is tested by an enamel conductometer. The aluminium tubes are filled with an electrolyte solution up to a fixed level at its open end. One electrode is connected to the tube nozzle, the second electrode is dipped into the solution. A defined voltage is applied for a fixed time. The induced current is a measure for the quality (pores and/or film thickness) of the internal coating.