WL 1.6974-100
Aerospace; high-strength hardened and tempered nickel-cobalt steel with approx. 0,3 C, 8 Ni, 4,5 Co, 1 Cr, 1 Mo, consumable electrode remelted; bars and forgings; design and production data, conversion
Edition
1992-08
WL 1.7736-1
Aerospace series - Weldable hardened and tempered chromium-molybdenum-vanadium steel, with approx. 0,15 C - 1,4 Cr - 0,9 Mo - 0,25 V - Part 1: Remelted with consumable electrode - Plate
Edition
2012-10
WL 1.7736-2
Aerospace series - Weldable hardened and tempered chromium-molybdenum-vanadium steel, with approx. 0,15 C - 1,4 Cr - 0,3 Mo - 0,25 V - Part 2: Remelted with consumable electrode - Bar and forging
Edition
2012-10
WL 1.7736-100
Aerospace series - Weldable hardened and tempered chromium-molybdenum-vanaduim steel with approx. 0,15 C - 1,4 Cr - 0,9 Mo - 0,25 V - Part 100: Consumable elektrode remelted - Plate, bar and forging - Design and production data, cross-referencing
Edition
2012-10
WL 2.4631-1
Aerospace; heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 2,3 Ti - 1,4 Al, consumable electrode remelted; sheet and strip
Edition
1993-08
WL 2.4631-2
Aerospace; heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 2,3 Ti - 1,4 Al, consumable electrode remelted; bars and forgings
Edition
1993-08
WL 2.4632-1
Aerospace; heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 18 Co - 2,5 Ti - 1,5 Al, consumable electrode remelted; sheet and strip
Edition
1993-08
WL 2.4632-2
Aerospace; heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 18 Co - 2,5 Ti - 1,5 Al, consumable electrode remelted; bars and forgings
Edition
1993-08
WL 2.4632-2 Berichtigung 1
Aerospace - Heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 18 Co - 2,5 Ti - 1,5 Al, consumable electrode remelted - Part 2: Bars and forgings, Corrigendum to WL 2.4632-2:1993-08
Edition
2019-04
WL 2.4632-3
Aerospace; heat-resisting nickel alloy with approx. 0,1 C - 20 Cr - 18 Co - 2,5 Ti - 1,5 Al, consumable electrode remelted; tubes
Edition