BS 3TA 2

Specification for sheet and strip of commercially pure titanium (tensile strength 390-540 MPa)
Edition 2009-11-30

Standards [CURRENT]

BS 3TA 6

Specification for sheet and strip of commercially pure titanium (tensile strength 570-730 MPa)
Edition 2009-11-30

Standards [CURRENT]

BS 3TA 10

Specification for sheet of titanium-aluminium-vanadium alloy (tensile strength 960-1270 MPa)
Edition 2009-11-30

Standards [CURRENT]

BS 3TA 21

Specification for sheet and strip of titanium-copper alloy (tensile strength 540-700 MPa)
Edition 2009-11-30

Standards [CURRENT]

BS 6L 16

Specification for sheet and strip of 99% aluminium (temper designation H14 or H24)
Edition 1985-12-31

Standards [CURRENT]

BS 6L 17

Specification for sheet and strip of 99% aluminium (temper designation-O)
Edition 1985-12-31

Draft standard

20/30420958 DC

BS EN 4890. Aerospace series. Steel X4CrNiMo16-5-1. Air melted. Hardened and tempered. Sheets. 0,3 mm = a = 6 mm. 900 MPa = Rm = 1050 MPa
Edition 2020-05-28

Draft standard

20/30425162 DC

BS EN 2467. Aerospace series. Steel X2CrNi18-9 (1.4307). Air melted. Softened. Plates, sheets and strips. 0,4 mm ≤ a ≤ 20 mm - 520 MPa ≤ R<(Index)m> ≤ 670 MPa
Edition 2020-09-10

Draft standard

20/30425168 DC

BS EN 3488. Aerospace series. Steel X6CrNiTi18-10 (1.4541). Air melted. Softened. Sheets and strips. a ≤ 6 mm - 500 MPa ≤ R<(Index)m> ≤ 700 MPa
Edition 2020-09-17

Draft standard

21/30442582 DC

BS EN 3361. Aerospace series. Steel X5CrNiCu15 5 (1.4545). Consumable electrode remelted. Solution treated and precipitation treated. Sheets and strips. a ≤ 6 mm - 1070 MPa ≤ R<(Index)m> ≤ 1220 MPa
Edition 2021-09-16