ASD-STAN prEN 2467

Aerospace series - Steel X2CrNi18-9 (1.4307) - Air melted - Softened - Plates, sheets and strips - 0,4 mm < = a < = 20 mm - 520 MPa < = Rₘ < = 670 MPa
Edition 2023-09-01

Technical rule [CURRENT]

ASD-STAN prEN 3487

Aerospace series - Steel X6CrNiTi18-10 (1.4541) - Air melted - Softened - Bars for machining - a or D ≤ 250 mm - 500 MPa ≤ Rₘ ≤ 700 MPa
Edition 2023-09-01

Technical rule [CURRENT]

ASD-STAN prEN 4630+CORR

Aerospace series - Steel X4CrNiMo16-5-1 (1.4418) - Air melted - Hardened and tempered - Forgings - Dₑ ≤ 200 mm - 900 MPa ≤ Rₘ ≤ 1050 MPa
Edition 2023-10-01

Technical rule [CURRENT]

ASD-STAN prEN 4631+CORR

Aerospace series - Steel X4CrNiMo16-5-1 (1.4418) - Air melted - Hardened and tempered - Bars - Dₑ ≤ 200 mm - 900 MPa ≤ Rₘ ≤ 1050 MPa
Edition 2023-10-01

Technical rule [CURRENT]

ASD-STAN prEN 3680

Steel FE-PA3601 (X6CrNiTi18-10) - Air melted - Solution treated - Seamless tubes for pressure applications - D ≤ 50 mm ; 0,5 mm ≤ a ≤ 5mm - 500 MPa ≤ Rm ≤ 750 MPa
Edition 1997-12-31

Technical rule [CURRENT]

ASD-STAN prEN 4090

Steel FE-PL5101 (13MoCrNiV4-4-3-1) - Vacuum induction melted and vacuum arc remelted - Carburized, hardened,sub-zero treated and tempered - Forgings - De ≤ 30 mm -- 1315 MPa ≤ Rm ≤ 1650 MPa
Edition 1997-11-28

Technical rule [New]

ASD-STAN prEN 3523+CORR

Aerospace series - Steel 15CrMoV6 (1.7334) - Air melted - Hardened and tempered - Bars for machining - Dₑ ≤ 100 mm - 1080 MPa ≤ Rₘ ≤ 1280 MPa
Edition 2024-05-23

Technical rule [CURRENT]

ASD-STAN prEN 4088

Steel FE-PL5101 (13MoCrNiV4-4-3-1) - Vacuum induction melted and vacuum arc remelted - Carburized, hardened,sub-zero treated and tempered - Bar for machining - De ≤ 30 mm - 1315 MPa ≤ Rm ≤ 1650 MPa
Edition 1997-11-28

Standards [CURRENT]

ISO 1133-2

Plastics - Determination of the melt mass-flow rate (MFR) and melt volume-flow rate (MVR) of thermoplastics - Part 2: Method for materials sensitive to time-temperature history and/or moisture
Edition 2011-12

Administrative provision

EU 2018/742

Commission Delegated Directive (EU) 2018/742 of 1 March 2018 amending, for the purposes of adapting to scientific and technical progress, Annex III to Directive 2011/65/EU of the European Parliament and of the Council as regards an exemption for lead in high melting temperature solders
Edition 2018-03-01

Related searches

Choose a keyword to learn more:
TOP