Standards [CURRENT]

SAE AMS 5706N

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated
Edition 2020-08-04

Standards [CURRENT]

SAE AMS 5707P

Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Edition 2023-03-23

Standards [CURRENT]

SAE AMS 5708M

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, and Rings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated
Edition 2019-01-04

Standards [CURRENT]

SAE AMS 5709J

Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution, Stabilization, and Precipitation Heat Treated
Edition 2019-09-04

Standards [CURRENT]

SAE AMS 5726F

Steel, Corrosion- and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability
Edition 2023-03-20

Standards [CURRENT]

SAE AMS 5731M

Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated Precipitation Hardenable
Edition 2023-09-05

Standards [CURRENT]

SAE AMS 5732K

Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1800 °F (982 °C) Solution and Precipitation Heat Treated
Edition 2023-11-15

Standards [CURRENT]

SAE AMS 5734L

Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
Edition 2024-04-10

Standards [CURRENT]

SAE AMS 5737R

Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1650 °F (899 °C) Solution and Precipitation Heat Treated
Edition 2023-09-07

Standards [CURRENT]

SAE AMS 5743K

Steel, Corrosion and Heat-Resistant, Bars and Forgings 15.5Cr - 4.5Ni - 2.9Mo - 0.10N Consumable Electrode Remelted Solution Heat Treated, Sub-Zero Cooled, Equalized, and Over-Tempered