Thermoplastics pipes and fittings - Vicat softening temperature: General test method and test conditions for Vinyl chloride - based (PVC-U, PVC-C, PVC-Hi) and Acryl nitrile - based (ABS, ASA) Pipes and Fittings
Abstract
The method specified is based on determining the temperature at which a standard indenter, under a force of 50 N ± 1 N, penetrates 1 mm into the surface of a test piece cut from the wall of a pipe or fitting while the temperature is raised at a constant rate. Is applicable only to thermoplastics materials for which it is possible to measure the temperature at which the rate of softening becomes rapid. Is based on ISO 306:1994 which, however, applies to materials in the form of sheets.
Begin
2024-02-16
WI
00155A1G
Planned document number
prEN ISO 2507 rev
Responsible national committee
NA 054-05-02 AA - Test methods for plastic pipes
Responsible european committee
CEN/TC 155 - Plastics piping systems and ducting systems
previous edition(s)
Order from DIN MediaThermoplastics pipes and fittings - Vicat softening temperature - Part 2: Test conditions for unplasticized poly(vinyl chloride) (PVC-U) or chlorinated poly(vinyl chloride) (PVC-C) pipes and fittings and for high impact resistance poly (vinyl chloride) (PVC-HI) pipes (ISO 2507-2:1995)
2017-10
Order from DIN Media
Thermoplastics pipes and fittings - Vicat softening temperature - Part 1: General test method (ISO 2507-1:1995)
2017-10
Order from DIN Media